Comal cracked during firing.
Small stress fractures formed during the firing compromising the functionality but not the form.
Micaceous clay crafted from start to finish by hand
12” x 12” x 1.5”
Care and use instructions here
Comal cracked during firing.
Small stress fractures formed during the firing compromising the functionality but not the form.
Micaceous clay crafted from start to finish by hand
12” x 12” x 1.5”
Care and use instructions here